Dynacron
Dynacron ProcessServicesProduct ApplicationsTechnical DataIndustry Specifications NEWSCONTACTLINKS

Composition:

Modified tungsten disulfide (WS2) in lamellar form

Hardness:

1.0-1.5 Moh’s scale

Molecular Weight:

248.02

Appearance:

Metallic silver when first applied, burnishing changes to polished rhodium

Co-efficient of Friction:

0.030, inclined plane method

Adhesion:

Mechanical molecular interlock

Carrier:

Dry air, no binder or adhesives

Curing:

No cure time required, applied at ambient temperature

Thickness:

0.000020 In. (1/2 micron) or less

Density:

7.4 gms/cc

Substrates:

All metal and plated surfaces, glass, fiberglass, rubber, porcelain and man-made surfaces

Temperature Range:

-188° to +538° C (-350° to +1000° F) in normal atmosphere, up to +1316° C (+2400° F) in a vacuum of 10-14 Torr

Chemical Stability:

Inert, non-toxic, corrosion resistant

Corrosion Resistance:

Minor delay of corrosion, will not inhibit eventual corrosion

Lox Compatibility:

Insensitive to detonation by, or in the presence of liquid oxygen

Load Capacity:

Same as substrate, up to 350,000 psi

Magnetism:

Non-magnetic

Vacuum Environment:

10-14 Torr

Degradation:

Will not cause distortive stress relief, additional stresses, or degradation to any surface

As a Substrate:

Accepts most paints, all platings, and is compatible with solvents, fuels and oils


Copyright © SCCS Industries LLC.

SCCS Industries LLC dba: Dynacron LLC • 900 South Cicero Avenue, Chicago IL 60644 USA
phone: 773-378-0736 • e-mail: info@dynacron.com

Bearings & GearsMedical/DentalValve, Pump & Mechanical ComponentsAerospace/Aircraft Tooling & Cutting DiesInjection MoldingAutomotive